Vapors

Longitudinal Velocity

cm/µs

in/µs

Alcohol Vapor (0° C)

.0231

.0091

Ether Vapor (0° C)

.0179

.007

Water Vapor (0° C)

.0401

.0158

Water Vapor (100° C)

.0405

.0159

Water Vapor (130° C)

.0424

.0167

Data compiled by Xactex Corporation.  Sources of original data are unknown.

-