  Shear(SV) at 45ƒ              Interface Radius of curvature in inches
  _______________________________________________________________________________________
  5.00 MHz (0.375" dia.)        0.50 0.63 0.75 0.88 1.00 1.12 1.25 1.38 1.50 2.25 3.00 6.00 
    


   FBH           ---------------------Curvature Correction Factors (dB)---------------------------------------
  DEPTH   DAC    0.50"    0.63"   0.75"   0.88"   1.00"   1.12"   1.25"   1.38"   1.50"  2.25"    3.00"   6.00"
  (in.)   (dB)   radius   radius  radius  radius  radius  radius  radius  radius  radius  radius  radius  radius
  ___________________________________________________________________________________________________________
  0.00    0.00    0.00    0.00    0.00    0.00    0.00    0.00    0.00    0.00    0.00    0.00    0.00    0.00
  0.10   -0.38   -2.65   -1.84   -1.67   -1.41   -1.22   -1.08   -0.97   -0.87   -0.80   -0.52   -0.39   -0.19
  0.20   -0.84   -6.12   -3.96   -3.56   -2.94   -2.53   -2.23   -1.97   -1.76   -1.61   -1.04   -0.77   -0.38
  0.30   -1.48  -11.08   -6.58   -5.85   -4.75   -4.05   -3.53   -3.09   -2.76   -2.51   -1.60   -1.17   -0.57
  0.40   -2.11  -16.19   -9.58   -8.37   -6.63   -5.55   -4.76   -4.11   -3.64   -3.29   -2.04   -1.48   -0.71
  0.50   -2.82   -5.14  -12.75  -11.16   -8.65   -7.14   -6.09   -5.25   -4.63   -4.19   -2.61   -1.89   -0.89
  0.60   -3.46   -1.10  -13.00  -13.12  -10.53   -8.66   -7.33   -6.31   -5.53   -4.94   -2.99   -2.14   -1.02
  0.70   -4.19    2.28   -5.44   -9.71  -11.96  -10.14   -8.59   -7.37   -6.42   -5.74   -3.49   -2.47   -1.17
  0.80   -4.86    3.43   -2.16   -3.89  -11.32  -11.08   -9.62   -8.28   -7.23   -6.49   -3.86   -2.79   -1.30
  0.90   -5.50    4.22    0.02   -1.53   -5.08  -11.00  -10.31   -9.04   -7.95   -7.09   -4.21   -2.99   -1.41
  1.00   -6.14    4.99    1.10    0.21   -3.06   -8.52  -10.40   -9.56   -8.50   -7.64   -4.58   -3.23   -1.47
  1.10   -6.81    5.70    2.78    1.57   -1.21   -3.17   -9.43   -9.78   -8.97   -8.17   -4.92   -3.52   -1.61
  1.20   -7.42    6.43    4.42    2.12    0.11   -2.68   -6.54   -9.41   -9.14   -8.46   -5.20   -3.67   -1.71
  1.30   -8.04    7.09    5.43    3.35    1.17   -0.90   -2.60   -8.29   -9.09   -8.66   -5.47   -3.87   -1.82
  1.40   -8.60    7.67    6.20    4.71    2.03    0.23   -1.76   -6.11   -8.59   -8.63   -5.65   -4.03   -1.83
  1.50   -9.17    8.15    6.77    5.64    3.01    1.09   -0.77   -3.07   -7.62   -8.34   -5.84   -4.17   -1.90
  1.60   -9.74    8.58    7.22    6.35    3.50    1.86    0.10   -1.04   -6.05   -7.85   -6.02   -4.31   -1.97
  1.70  -10.31    8.96    7.59    6.90    3.75    2.40    0.76   -0.93   -4.06   -7.12   -6.18   -4.45   -2.06
  1.80  -10.83    9.35    7.95    7.38    4.25    3.06    1.40   -0.55   -1.77   -5.91   -6.27   -4.56   -2.12
  1.90  -11.34    9.71    8.28    7.78    4.85    3.54    2.11    0.51   -0.41   -4.51   -6.35   -4.65   -2.16
  2.00  -11.85   10.04    8.56    8.12    5.49    4.10    2.53    0.95   -0.08   -2.74   -6.40   -4.72   -2.19
  2.10  -12.34   10.34    8.83    8.42    6.08    4.54    3.07    1.47   -0.29   -1.07   -6.43   -4.82   -2.25
  2.20  -12.80   10.65    9.11    8.71    6.65    4.92    3.43    2.03    0.24    0.02   -6.43   -4.86   -2.28
  2.30  -13.26   10.93    9.36    8.98    7.14    5.14    3.90    2.40    1.14    0.51   -6.38   -4.91   -2.30
  2.40  -13.71   11.19    9.59    9.22    7.53    5.29    4.28    2.85    1.48    0.57   -6.33   -4.96   -2.32
  2.50  -14.16   11.42    9.80    9.44    7.88    5.45    4.52    3.24    1.78    0.36   -6.25   -4.99   -2.38
  2.60  -14.60   11.62    9.99    9.63    8.19    5.63    4.75    3.44    2.22    0.59   -6.21   -5.01   -2.42
  2.70  -15.04   11.79   10.16    9.82    8.44    5.84    5.02    3.77    2.52    1.26   -6.11   -5.06   -2.46
  2.80  -15.47   11.95   10.32    9.98    8.68    6.09    5.32    4.09    2.83    1.76   -5.97   -5.09   -2.49
  2.90  -15.86   12.12   10.50   10.17    8.91    6.37    5.61    4.28    3.13    2.04   -5.82   -5.09   -2.49
  3.00  -16.25   12.27   10.67   10.34    9.12    6.66    5.86    4.45    3.33    2.24   -5.67   -5.12   -2.49
  3.10  -16.64   12.42   10.81   10.49    9.32    6.95    6.05    4.68    3.53    2.50   -5.51   -5.12   -2.52
  3.20  -17.02   12.56   10.94   10.63    9.49    7.23    6.19    4.92    3.80    2.79   -5.30   -5.10   -2.54
  3.30  -17.40   12.69   11.05   10.76    9.65    7.50    6.30    5.14    4.04    3.03   -5.05   -5.06   -2.56
  3.40  -17.77   12.81   11.16   10.88    9.80    7.74    6.39    5.30    4.18    3.20   -4.84   -5.07   -2.58
  3.50  -18.14   12.93   11.26   10.98    9.93    7.96    6.46    5.43    4.28    3.37   -4.62   -5.06   -2.59
  3.60  -18.49   13.04   11.36   11.08   10.07    8.18    6.55    5.55    4.44    3.56   -4.40   -5.03   -2.61
  3.70  -18.82   13.17   11.47   11.19   10.21    8.40    6.64    5.68    4.66    3.77   -4.14   -5.00   -2.62
  3.80  -19.15   13.28   11.57   11.30   10.33    8.60    6.74    5.82    4.88    3.94   -3.85   -4.99   -2.64
  3.90  -19.48   13.39   11.67   11.40   10.45    8.77    6.84    5.98    5.05    4.06   -3.54   -4.96   -2.65
  4.00  -19.80   13.49   11.76   11.49   10.56    8.93    6.94    6.14    5.17    4.17   -3.22   -4.92   -2.66
  4.10  -20.12   13.59   11.85   11.58   10.67    9.08    7.05    6.30    5.27    4.31   -2.92   -4.87   -2.67
  4.20  -20.44   13.68   11.93   11.66   10.76    9.23    7.16    6.46    5.36    4.48   -2.63   -4.81   -2.67
  4.30  -20.75   13.77   12.01   11.74   10.86    9.36    7.27    6.62    5.46    4.65   -2.36   -4.77   -2.67
  4.40  -21.05   13.85   12.08   11.81   10.94    9.49    7.39    6.75    5.57    4.80   -2.07   -4.74   -2.67
  4.50  -21.35   13.93   12.15   11.88   11.02    9.60    7.50    6.86    5.69    4.91   -1.77   -4.70   -2.67
  4.60  -21.65   14.01   12.22   11.95   11.10    9.72    7.60    6.96    5.81    4.98   -1.47   -4.65   -2.68
  4.70  -21.94   14.08   12.28   12.01   11.17    9.82    7.70    7.06    5.94    5.04   -1.16   -4.59   -2.69
  4.80  -22.23   14.15   12.34   12.07   11.24    9.92    7.80    7.15    6.05    5.10   -0.85   -4.57   -2.71
  4.90  -22.52   14.21   12.40   12.13   11.31   10.02    7.89    7.24    6.15    5.18   -0.54   -4.54   -2.72
  5.00  -22.80   14.27   12.46   12.18   11.37   10.10    7.99    7.32    6.25    5.28   -0.24   -4.51   -2.73
  5.10  -23.08   14.33   12.51   12.23   11.43   10.19    8.08    7.39    6.33    5.39    0.06   -4.47   -2.74
  5.20  -23.35   14.40   12.57   12.29   11.49   10.28    8.18    7.47    6.41    5.51    0.36   -4.41   -2.74
  5.30  -23.61   14.46   12.63   12.35   11.56   10.37    8.28    7.55    6.50    5.63    0.65   -4.35   -2.73
  5.40  -23.87   14.53   12.69   12.41   11.62   10.45    8.38    7.62    6.57    5.73    0.94   -4.28   -2.73
  5.50  -24.12   14.59   12.74   12.46   11.68   10.53    8.47    7.69    6.64    5.82    1.19   -4.21   -2.72
  5.60  -24.37   14.64   12.80   12.51   11.74   10.60    8.57    7.75    6.71    5.90    1.41   -4.14   -2.71
  5.70  -24.62   14.70   12.85   12.56   11.79   10.67    8.65    7.81    6.77    5.97    1.61   -4.08   -2.72
  5.80  -24.86   14.75   12.90   12.61   11.84   10.73    8.73    7.86    6.83    6.03    1.80   -4.03   -2.72
  5.90  -25.10   14.81   12.94   12.65   11.89   10.80    8.81    7.90    6.88    6.09    1.98   -3.98   -2.73
  6.00  -25.34   14.86   12.99   12.70   11.94   10.86    8.89    7.94    6.94    6.15    2.15   -3.92   -2.73
  6.10  -25.58   14.90   13.03   12.74   11.99   10.91    8.96    7.97    7.00    6.20    2.30   -3.86   -2.74
  6.20  -25.81   14.95   13.08   12.78   12.03   10.97    9.03    8.00    7.06    6.24    2.44   -3.80   -2.74
  6.30  -26.04   14.99   13.12   12.82   12.08   11.02    9.10    8.03    7.12    6.28    2.57   -3.75   -2.75
  6.40  -26.27   15.04   13.16   12.86   12.12   11.07    9.17    8.06    7.18    6.33    2.68   -3.71   -2.75
  6.50  -26.49   15.08   13.19   12.89   12.16   11.12    9.23    8.09    7.23    6.37    2.79   -3.66   -2.76
  6.60  -26.72   15.12   13.23   12.93   12.19   11.17    9.30    8.11    7.29    6.42    2.88   -3.62   -2.76
  6.70  -26.94   15.16   13.27   12.96   12.23   11.22    9.36    8.14    7.35    6.47    2.97   -3.57   -2.76
  6.80  -27.16   15.19   13.30   13.00   12.27   11.26    9.42    8.16    7.41    6.52    3.04   -3.52   -2.76
  6.90  -27.37   15.23   13.33   13.03   12.30   11.30    9.47    8.19    7.46    6.57    3.10   -3.46   -2.76
  7.00  -27.59   15.26   13.37   13.06   12.33   11.34    9.53    8.21    7.52    6.62    3.16   -3.41   -2.77
  7.10  -27.80   15.30   13.40   13.09   12.36   11.38    9.59    8.24    7.57    6.68    3.21   -3.35   -2.77
  7.20  -28.00   15.33   13.43   13.12   12.40   11.42    9.64    8.26    7.62    6.73    3.25   -3.30   -2.77
  7.30  -28.21   15.35   13.46   13.15   12.42   11.45    9.69    8.28    7.67    6.78    3.29   -3.24   -2.77
  7.40  -28.41   15.38   13.49   13.18   12.46   11.49    9.74    8.31    7.73    6.83    3.32   -3.18   -2.76
  7.50  -28.61   15.42   13.52   13.21   12.49   11.53    9.80    8.34    7.78    6.89    3.35   -3.11   -2.76
  7.60  -28.80   15.45   13.55   13.24   12.52   11.57    9.85    8.37    7.84    6.95    3.38   -3.04   -2.75
  7.70  -28.99   15.48   13.58   13.27   12.56   11.61    9.90    8.40    7.88    7.00    3.40   -2.98   -2.74
  7.80  -29.18   15.51   13.62   13.30   12.59   11.64    9.95    8.42    7.93    7.05    3.42   -2.91   -2.74
  7.90  -29.37   15.54   13.65   13.33   12.62   11.68   10.00    8.45    7.98    7.10    3.43   -2.85   -2.74
  8.00  -29.56   15.57   13.68   13.36   12.65   11.71   10.05    8.47    8.02    7.14    3.45   -2.79   -2.74
  8.10  -29.74   15.60   13.70   13.39   12.68   11.75   10.10    8.50    8.06    7.19    3.46   -2.74   -2.74
  8.20  -29.92   15.62   13.73   13.41   12.70   11.78   10.14    8.52    8.09    7.23    3.47   -2.68   -2.74
  8.30  -30.10   15.65   13.76   13.44   12.73   11.81   10.18    8.54    8.13    7.27    3.48   -2.63   -2.74
  8.40  -30.28   15.68   13.79   13.47   12.76   11.84   10.23    8.57    8.16    7.30    3.48   -2.57   -2.74
  8.50  -30.46   15.70   13.81   13.49   12.78   11.87   10.27    8.59    8.20    7.34    3.49   -2.52   -2.74
  8.60  -30.64   15.73   13.84   13.52   12.81   11.90   10.31    8.61    8.23    7.37    3.49   -2.46   -2.74
  8.70  -30.81   15.75   13.86   13.54   12.83   11.93   10.35    8.63    8.26    7.40    3.50   -2.41   -2.74
  8.80  -30.98   15.77   13.88   13.56   12.86   11.95   10.39    8.66    8.29    7.43    3.48   -2.36   -2.74
  8.90  -31.15   15.80   13.91   13.58   12.88   11.98   10.42    8.68    8.32    7.46    3.46   -2.32   -2.74
  9.00  -31.32   15.82   13.93   13.61   12.90   12.01   10.46    8.70    8.35    7.48    3.44   -2.27   -2.73
  9.10  -31.49   15.84   13.95   13.63   12.93   12.03   10.50    8.72    8.38    7.51    3.42   -2.23   -2.73
  9.20  -31.66   15.86   13.97   13.65   12.95   12.05   10.53    8.74    8.40    7.53    3.41   -2.18   -2.73
  9.30  -31.82   15.88   14.00   13.67   12.97   12.08   10.57    8.76    8.43    7.56    3.39   -2.14   -2.73
  9.40  -31.98   15.89   14.02   13.69   12.99   12.10   10.60    8.79    8.45    7.58    3.38   -2.09   -2.73
  9.50  -32.15   15.91   14.04   13.71   13.01   12.12   10.63    8.81    8.48    7.60    3.37   -2.05   -2.72
  9.60  -32.31   15.93   14.06   13.73   13.03   12.15   10.66    8.83    8.50    7.62    3.36   -2.00   -2.72
  9.70  -32.47   15.94   14.08   13.75   13.05   12.17   10.69    8.85    8.52    7.64    3.36   -1.96   -2.72
  9.80  -32.62   15.96   14.09   13.77   13.07   12.19   10.72    8.87    8.55    7.66    3.35   -1.91   -2.71
  9.90  -32.78   15.98   14.11   13.78   13.09   12.21   10.75    8.89    8.57    7.68    3.35   -1.87   -2.71
 10.00  -32.94   15.99   14.13   13.80   13.10   12.23   10.78    8.91    8.59    7.70    3.35   -1.82   -2.71
 10.10  -33.09   16.01   14.15   13.82   13.12   12.25   10.81    8.93    8.61    7.72    3.36   -1.77   -2.70
 10.20  -33.24   16.02   14.17   13.84   13.14   12.27   10.83    8.94    8.63    7.73    3.36   -1.73   -2.70
 10.30  -33.39   16.04   14.18   13.85   13.16   12.29   10.85    8.96    8.65    7.75    3.37   -1.68   -2.70
 10.40  -33.54   16.05   14.20   13.87   13.17   12.31   10.88    8.98    8.67    7.77    3.38   -1.64   -2.69
 10.50  -33.69   16.06   14.22   13.88   13.19   12.32   10.90    9.00    8.69    7.78    3.39   -1.59   -2.70
 10.60  -33.84   16.08   14.23   13.90   13.20   12.34   10.92    9.02    8.71    7.80    3.40   -1.55   -2.70
 10.70  -33.99   16.09   14.25   13.91   13.22   12.36   10.94    9.04    8.72    7.82    3.42   -1.50   -2.70
 10.80  -34.13   16.11   14.26   13.93   13.23   12.37   10.96    9.06    8.74    7.83    3.44   -1.46   -2.70
 10.90  -34.27   16.12   14.28   13.94   13.25   12.39   10.98    9.07    8.76    7.85    3.46   -1.41   -2.70
 11.00  -34.42   16.13   14.29   13.96   13.26   12.41   11.00    9.09    8.77    7.86    3.48   -1.37   -2.70