Partial
List of AWS Specifications
Please note that this list of ISO specifications
is provided for general reference only and may not be complete
or current. Reference to the release date of the specification
has been intentionally left off so that this list will not be
used to check for the latest version of the document. Information
provided by ISO should be consulted to ensure accuracy. The ISO
web site can be found at www.iso.org
19.100 Non-destructive testing
-
ISO/TTA 3, Polycrystalline materials -- Determination
of residual stresses by neutron diffraction.
-
ISO 1027, Radiographic image quality indicators
for non-destructive testing -- Principles and identification.
-
ISO 3057, Non-destructive testing -- Metallographic
replica techniques of surface examination.
-
ISO 3058, Non-destructive testing -- Aids to
visual inspection -- Selection of low-power magnifiers.
-
ISO 3059, Non-destructive testing -- Penetrant
testing and magnetic particle testing - Viewing conditions.
-
ISO 3452, Non-destructive testing -- Penetrant
inspection --General principles.
-
ISO 3452-2, Non-destructive testing -- Penetrant testing -- Part
2: Testing of penetrant materials.
- ISO 3452-3, Non-destructive testing -- Penetrant testing --
Part 3: Reference test blocks.
- ISO 3452-4, Non-destructive testing -- Penetrant testing --
Part 4: Equipment.
- ISO 3453, Non-destructive testing -- Liquid penetrant inspection
-- Means of verification.
- ISO 3999, Apparatus for gamma radiography -- Specification.
- ISO 3999-1, Radiation protection -- Apparatus for industrial
gamma radiography -- Part 1: Specifications for performance, design
and tests.
-
ISO 5576, Non-destructive testing -- Industrial
X-ray and gamma-ray radiology -- Vocabulary.
- ISO 5577, Non-destructive testing -- Ultrasonic inspection
-- Vocabulary.
- ISO 5580, Non-destructive testing -- Industrial radiographic
illuminators -- Minimum requirements.
- ISO 9712, Non-destructive testing -- Qualification and certification
of personnel.
- ISO 9934-1, Non-destructive testing -- Magnetic particle testing
-- Part 1: General principles.
- ISO 9934-3, Non-destructive testing -- Magnetic particle testing
-- Part 3: Equipment.
- ISO 9935, Non-destructive testing -- Penetrant flaw detectors
-- General technical requirements.
- ISO 10375, Non-destructive testing -- Ultrasonic inspection
- - Characterization of search unit and sound field.
- ISO 11537, Non-destructive testing -- Thermal neutron radiographic
testing -- General principles and basic rules.
- ISO 12706, Non-destructive testing -- Terminology - Terms used
in penetrant testing.
- ISO 12710, Non-destructive testing -- Ultrasonic inspection
--Evaluating electronic characteristics of ultrasonic test instruments.
- ISO 12713, Non-destructive testing -- Acoustic emission inspection
-- Primary calibration of transducers.
- ISO 12714, Non-destructive testing -- Acoustic emission inspection
-- Secondary calibration of acoustic emission sensors.
- ISO 12715, Ultrasonic non-destructive testing -- Reference blocks
and test procedures for the characterization of contact search
unit beam profiles.
- ISO 12716, Non-destructive testing -- Acoustic emission inspection
-- Vocabulary.
- ISO 12721, Non-destructive testing -- Thermal neutron radiographic
testing -- Determination of beam L/D ratio.
- ISO 15708-1, Non-destructive testing -- Radiation methods --
Computed tomography -- Part 1: Principles.
- ISO 15708-2, Non-destructive testing -- Radiation methods --
Computed tomography -- Part 2: Examination practices.
37.040.25 Radiographic films.
- ISO 11699-1, Non-destructive testing -- Industrial radiographic
films -- Part 1: Classification of film systems for industrial
radiography.
- ISO 11699-2, Non-destructive testing -- Industrial radiographic
films -- Part 2: Control of film processing by means of reference
values.
77.040.20 Non-destructive testing of metals.
- ISO 4986, Steel castings -- Magnetic particle inspection.
- ISO 4987, Steel castings -- Penetrant inspection.
- ISO 4993, Steel castings -- Radiographic inspection.
- ISO 5579, Non-destructive testing -- Radiographic examination
of metallic materials by X- and gamma rays -- Basic rules.
- ISO 5948, Railway rolling stock material -- Ultrasonic acceptance
testing.
- ISO 6933, Railway rolling stock material -- Magnetic particle
acceptance testing.
- ISO 9302, Seamless and welded (except submerged arc-welded)
steel tubes for pressure purposes -- electromagnetic testing for
verification of hydraulic leak-tightness.
- ISO 9303, Seamless and welded (except submerged arc-welded)
steel tubes for pressure purposes -- Full peripheral ultrasonic
testing for the detection of longitudinal imperfections.
- ISO 9304, Seamless and welded (except submerged arc-welded)
steel tubes for pressure purposes -- Eddy current testing for
the detection of imperfections.
- ISO 9305, Seamless steel tubes for pressure purposes -- Full
peripheral ultrasonic testing for the detection of transverse
imperfections.
- ISO 9402, Seamless and welded (except submerged arc-welded)
steel tubes for pressure purposes -- Full peripheral magnetic
transducer/flux leakage testing of ferromagnetic steel tubes for
the detection of longitudinal imperfections.
- ISO 9598, Seamless steel tubes for pressure purposes -- Full
peripheral magnetic transducer/flux leakage testing of ferromagnetic
steel tubes for the detection of transverse imperfections.
- ISO 9915, Aluminium alloy castings -- Radiography testing.
- ISO 9916, Aluminium alloy and magnesium alloy castings -- Liquid
penetrant inspection.
- ISO 10049, Aluminium alloy castings -- Visual method for assessing
the porosity.
- ISO 10124, Seamless and welded (except submerged arc-welded)
steel tubes for pressure purposes -- Ultrasonic testing for the
detection of laminar imperfections.
- ISO 10332, Seamless and welded (except submerged arc-welded)
steel tubes for pressure purposes -- Ultrasonic testing for the
verification of hydraulic leak-tightness.
- ISO 10543, Seamless and hot-stretch-reduced welded steel tubes
for pressure purposes -- Full peripheral ultrasonic thickness
testing.
- ISO 11484, Steel tubes for pressure purposes -- Qualification
and certification of non-destructive testing (NDT) personnel.
- ISO 11496, Seamless and welded steel tubes for pressure purposes
-- Ultrasonic testing of tube ends for the detection of laminar
imperfections.
- ISO 11971, Visual examination of surface quality of steel castings.
- ISO 12094, Welded steel tubes for pressure purposes -- Ultrasonic
testing for the detection of laminar imperfections in strips/plates
used in the manufacture of welded tubes.
- ISO 12095, Seamless and welded steel tubes for pressure purposes
-- Liquid penetrant testing.
- ISO 13664, Seamless and welded steel tubes for pressure purposes
-- Magnetic particle inspection of the tube ends for the detection
of laminar imperfections.
- ISO 13665, Seamless and welded steel tubes for pressure purposes
-- Magnetic particle inspection of the tube body for the detection
of surface imperfections.
25.160.40 Welded joints and welds Including welding position
and mechanical and non-destructive testing of welded joints.
- ISO 1106-1, Recommended practice for radiographic examination
of fusion welded joints -- Part 1: Fusion welded butt joints in
steel plates up to 50 mm thick.
- ISO 1106-2, Recommended practice for radiographic examination
of fusion welded joints -- Part 2: Fusion welded butt joints in
steel plates thicker than 50 mm and up to and including 200 mm
in thickness.
- ISO 1106-3, Recommended practice for radiographic examination
of fusion welded joints -- Part 3: Fusion welded circumferential
joints in steel pipes of up to 50 mm wall thickness.
- ISO 2400, Welds in steel -- Reference block for the calibration
of equipment for ultrasonic examination.
- ISO 2437, Recommended practice for the X-ray inspection of fusion
welded butt joints for aluminium and its alloys and magnesium
and its alloys 5 to 50 mm thick.
- ISO 2504, Radiography of welds and viewing conditions for films
-- Utilization of recommended patterns of image quality indicators
(I.Q.I.).
- ISO 5817, Arc-welded joints in steel -- Guidance on quality
levels for imperfections.
- ISO 6520-1, Welding and allied processes -- Classification of
geometric imperfections in metallic materials -- Part 1: Fusion
welding.
- ISO 6520-2, Welding and allied processes -- Classification of
geometric imperfections in metallic materials -- Part 2: Welding
with pressure.
- ISO 7963, Welds in steel -- Calibration block No. 2 for ultrasonic
examination of welds.
- ISO 9015-1, Destructive tests on welds in metallic materials
-- Hardness testing -- Part 1: Hardness test on arc welded joints.
- ISO 9764, Electric resistance and induction welded steel tubes
for pressure purposes -- Ultrasonic testing of the weld seam for
the detection of longitudinal imperfections.
- ISO 9765, Submerged arc-welded steel tubes for pressure purposes
-- Ultrasonic testing of the weld seam for the detection of longitudinal
and/or transverse imperfections.
- ISO 10042, Arc-welded joints in aluminium and its weldable alloys
--Guidance on quality levels for imperfections.
- ISO 12096, Submerged arc-welded steel tubes for pressure purposes
-- Radiographic testing of the weld seam for the detection of
imperfections.
- ISO 13663, Welded steel tubes for pressure purposes -- Ultrasonic
testing of the area adjacent to the weld seam for the detection
of laminar imperfections.
- ISO 13919-1, Welding -- Electron and laser-beam welded joints
-- Guidance on quality levels for imperfections -- Part 1: Steel.
- ISO 13919-2, Welding -- Electron and laser beam welded joints
-- Guidance on quality levels for imperfections -- Part 2: Aluminium