Partial
List of ASTM Specifications
Please note that this list of ASTM specifications
is provided for general reference only and may not be complete
or current. Reference to the release date of the specification
has been intentionally left off so that this list will not be
used to check for the latest version of the document. Information
provided by ASTM International should be consulted to ensure accuracy.
ASTM web site can be found at www.astm.org
-
A577/A577M, Standard Specification for Ultrasonic
Angle-Beam Examination of Steel Plates.
-
A578/A578M, Standard Specification for Straight-Beam
Ultrasonic Examination of Plain and Clad Steel Plates for Special
Applications.
-
A745/A745M, Standard Practice for Ultrasonic
Examination of Austenitic Steel Forgings.
-
A898/A898M, Standard Specification for Straight
Beam Ultrasonic Examination of Rolled Steel Structural Shapes.
-
A880, Standard Practice for Criteria for Use
in Evaluation of Testing Laboratories and Organizations for
Examination and Inspection of Steel, Stainless Steel, and Related
Alloys.
-
B 244, Measurement of Thickness of Anodic
Coatings on Aluminum and Other Nonconductive Coatings on Nonmagnetic
Basis Metals with Eddy-Current Instruments.
-
B 499, Measurement of Coating Thickness by
the Magnetic Method: Nonmagnetic Coatings on Magnetic Base
Metals.
-
B 457, Standard Test Method for Measurement
of Impedance of Anodic Coatings on Aluminum.
-
B 548, Standard Test Method for Ultrasonic
Inspection of Aluminum-Alloy Plate for Pressure Vessels.
-
B 594, Standard Practice for Ultrasonic Inspection
of Aluminum-Alloy Wrought Products for Aerospace Applications.
-
B 773, Standard Guide for Ultrasonic C-Scan
Bond Evaluation of Brazed or Welded Electrical Contact Assemblies.
-
C 1175, Standard Guide to Test Methods and
Standards for Nondestructive Testing of Advanced Ceramics.
-
C 1331, Standard Test Method for Measuring
Ultrasonic Velocity in Advanced Ceramics with Broadband Pulse-Echo
Cross-Correlation Method.
-
C 1332, Standard Test Method for Measurement
of Ultrasonic Attenuation Coefficients of Advanced Ceramics
by Pulse-Echo Contact Technique.
-
C 1383, Standard Test Method for Measuring
the P-Wave Speed and the Thickness of Concrete Plates Using
the Impact-Echo Method.
-
C 805, Standard Test Method for Rebound
Number of Hardened Concrete.
-
C 597, Standard Test Method for Pulse Velocity
Through Concrete.
-
D1186, Nondestructive Measurement of Dry
Film Thickness of Nonmagnetic Coatings Applied to a Ferrous
Base.
-
D1400, Nondestructive Measurement of Dry
Film Thickness of Nonconductive Coatings Applied to a Nonferrous
Metal Base.
-
D 4015, Standard Test Methods for Modulus
and Damping of Soils by the Resonant-Column Method.
-
D 4602, Standard Guide for Nondestructive
Testing of Pavements Using Cyclic-Loading Dynamic Deflection
Equipment.
-
D 5339, Standard Practice for Quality
Assurance Plan for Structural Steel Fabrication for Highway
Structures.
-
D 5641, Standard Practice for Geomembrane
Seam Evaluation by Vacuum Chamber.
-
D 5820, Standard Practice for Pressurized
Air Channel Evaluation of Dual Seamed Geomembranes.
-
D 5858, Standard Guide for Calculating
In Situ Equivalent Elastic Moduli of Pavement Materials
Using Layered Elastic Theory.
-
D 6087, Standard Test Method for Evaluating
Asphalt-Covered Concrete Bridge Decks Using Ground Penetrating
Radar.
-
D 6365, Standard Practice for the Nondestructive
Testing of Geomembrane Seams using the Spark Tests.
-
E 94, Standard Guide for Radiographic Examination.
-
E 114, Standard Practice for Ultrasonic Pulse-Echo
Straight-Beam Examination by the Contact Method.
- E 125, Standard Reference Photographs for Magnetic Particle
Indications on Ferrous Castings.
- E 127, Standard Practice for Fabricating and Checking Aluminum
Alloy Ultrasonic Standard Reference Blocks.
-
E 142, Standard Method for Controlling Quality
of Radiographic Testing.
-
E 155, Standard Reference Radiographs for Inspection
of Aluminum and Magnesium Castings.
-
E 164, Standard Practice for Ultrasonic Contact
Examination of Weldments.
-
E 165, Standard Test Method for Liquid Penetrant
Examination.
- E 186, Standard Reference Radiographs for Heavy-Walled (2 to
4 1/2-in. (51 to 114-mm)) Steel Castings.
- E 192, Standard Reference Radiographs for Investment Steel Castings
of Aerospace Applications.
-
E 213, Standard Practice for Ultrasonic Examination
of Metal Pipe and Tubing.
-
E 214, Standard Practice for Immersed Ultrasonic
Examination by the Reflection Method Using Pulsed Longitudinal
Waves.
-
E 215, Standard Practice for Standardizing Equipment
for Electromagnetic Examination of Seamless Aluminum-Alloy Tube.
- E 242, Standard Reference Radiographs for Appearances of Radiographic
Images as Certain Parameters Are Changed.
- E 243, Standard Practice for Electromagnetic (Eddy-Current)
Examination of Copper and Copper-Alloy Tubes.
- E272, Standard Reference Radiographs for High-Strength Copper-Base
and Nickel-Copper Alloy Castings.
- E 273, Standard Practice for Ultrasonic Examination of the Weld
Zone of Welded Pipe and Tubing.
- E 280, Standard Reference Radiographs for Heavy-Walled (4 1/2
to 12-in. (114 to 305-mm)) Steel Castings.
- E 309, Standard Practice for Eddy-Current Examination of Steel
Tubular Products Using Magnetic Saturation.
- E 310, Standard Reference Radiographs for Tin Bronze Castings.
- E 317, Standard Practice for Evaluating Performance Characteristics
of Ultrasonic Pulse- Echo Examination Instruments and Systems
Without the Use of Electronic Measurement Instruments.
-
E 329, Standard Specification for Agencies
Engaged in the Testing and/or Inspection of Materials Used in
Construction.
-
E 376, Standard Practice for Measuring Coating
Thickness by Magnetic-Field or Eddy-Current (Electromagnetic)
Test Methods.
- E 390, Standard Reference Radiographs for Steel Fusion Welds.
- E 408, Standard Test Methods for Total Normal Emittance of Surfaces
Using Inspection-Meter Techniques.
- E 426, Standard Practice for Electromagnetic (Eddy-Current)
Examination of Seamless and Welded Tubular Products, Austenitic
Stainless Steel and Similar Alloys.
- E 427, Standard Practice for Testing for Leaks Using the Halogen
Leak Detector (Alkali-Ion Diode).
- E 428, Standard Practice for Fabrication and Control of Steel
Reference Blocks Used in Ultrasonic Examination.
- E 431, Standard Guide to Interpretation of Radiographs of Semiconductors
and Related Devices.
- E 432, Standard Guide for Selection of a Leak Testing Method.
- E 433, Standard Reference Photographs for Liquid Penetrant Inspection.
- E 446, Standard Reference Radiographs for Steel Castings Up
to 2 in. (51 mm) in Thickness.
- E 479, Standard Guide for Preparation of a Leak Testing Specification.
- E 493, Standard Test Methods for Leaks Using the Mass Spectrometer
Leak Detector in the Inside-Out Testing Mode.
- E 494, Standard Practice for Measuring Ultrasonic Velocity in
Materials.
-
E 498, Standard Test Methods for Leaks Using
the Mass Spectrometer Leak Detector or Residual Gas Analyzer
in the Tracer Probe Mode.
-
E 499, Standard Test Methods for Leaks Using
the Mass Spectrometer Leak Detector in the Detector Probe Mode.
-
E 505, Standard Reference Radiographs for Inspection
of Aluminum and Magnesium Die Castings.
-
E 515, Standard Test Method for Leaks Using
Bubble Emission Techniques.
-
E 543, Standard Practice for Agencies Performing
Nondestructive Testing.
-
E 545, Standard Test Method for Determining
Image Quality in Direct Thermal Neutron Radiographic Examination.
-
E 566, Standard Practice for Electromagnetic
(Eddy-Current) Sorting of Ferrous Metals.
-
E 569, Standard Practice for Acoustic Emission
Monitoring of Structures During Controlled Stimulation.
-
E 570, Standard Practice for Flux Leakage Examination
of Ferromagnetic Steel Tubular Products.
-
E 571, Standard Practice for Electromagnetic
(Eddy-Current) Examination of Nickel and Nickel Alloy Tubular
Products.
-
E 587, Standard Practice for Ultrasonic Angle-Beam
Examination by the Contact Method.
-
E 588, Standard Practice for Detection of Large
Inclusions in Bearing Quality Steel by the Ultrasonic Method.
-
E 592, Standard Guide to Obtainable ASTM Equivalent
Penetrameter Sensitivity for Radiography of Steel Plates 1/4
to 2 in. (6 to 51 mm) Thick with X-Rays and 1 to 6 in. (25 to
152 mm) Thick with Cobalt-60.
- E 650, Standard Guide for Mounting Piezoelectric Acoustic Emission
Sensors.
- E 664, Standard Practice for the Measurement of the Apparent
Attenuation of Longitudinal Ultrasonic Waves by Immersion Method.
- E 689, Standard Reference Radiographs for Ductile Iron Castings.
- E 690, Standard Practice for In Situ Electromagnetic (Eddy-Current)
Examination of Nonmagnetic Heat Exchanger Tubes.
-
E 703, Standard Practice for Electromagnetic
(Eddy-Current) Sorting of Nonferrous Metals.
-
E 709 Standard Guide for Magnetic Particle Examination.
-
E 746, Standard Test Method for Determining
Relative Image Quality Response of Industrial Radiographic Film.
-
E 747, Standard Practice for Design, Manufacture,
and Material Grouping Classification of Wire Image
QualityIndicators (IQI) used for Radiology.
-
E 748, Standard Practices for Thermal Neutron
Radiography of Materials.
-
E 749, Standard Practice for Acoustic Emission
Monitoring During Continuous Welding.
-
E 750, Standard Practice for Characterizing
Acoustic Emission Instrumentation.
-
E 751, Standard Practice for Acoustic Emission
Monitoring During Resistance Spot-Welding.
-
E 797, Standard Practice for Measuring
Thickness by Manual Ultrasonic Pulse-Echo Contact Method.
-
E 801, Standard Practice for Controlling
Quality of Radiological Examination of Electronic Devices.
- E 802, Standard Reference Radiographs for Gray Iron Castings
Up to 4 1/2 in. (114 mm) in Thickness.
- E 803, Standard Test Method for Determining the L/D Ratio of
Neutron Radiography Beams.
- E 908, Standard Practice for Calibrating Gaseous Reference Leaks.
- E 976, Standard Guide for Determining the Reproducibility of
Acoustic Emission Sensor Response.
- E 977, Standard Practice for Thermoelectric Sorting of Electrically
Conductive Materials.
- E 998, Standard Test Method for Structural Performance of Glass
in Windows, Curtain Walls, and Doors Under the Influence of Uniform
Static Loads by Nondestructive Method.
- E 999, Standard Guide for Controlling the Quality of Industrial
Radiographic Film Processing.
- E 1001, Standard Practice for Detection and Evaluation of Discontinuities
by the Immersed Pulse-Echo Ultrasonic Method Using Longitudinal
Waves.
-
E 1002, Standard Test Method for Leaks Using
Ultrasonics.
-
E 1003, Standard Test Method for Hydrostatic
Leak Testing.
-
E 1004, Standard Practice for Determining Electrical
Conductivity Using the Electromagnetic (Eddy-Current) Method.
-
E 1025, Standard Practice for Design, Manufacture,
and Material Grouping Classification of Hole-Type Image Quality
Indicators (IQI) used for Radiology.
-
E 1030, Standard Test Method for Radiographic
Examination of Metallic Castings.
-
E 1032, Standard Test Method for Radiographic
Examination of Weldments.
- E 1033, Standard Practice for Electromagnetic (Eddy-Current)
Examination of Type F-Continuously Welded (CW) Ferromagnetic Pipe
and Tubing Above the Curie Temperature.
- E 1065, Standard Guide for Evaluating Characteristics of Ultrasonic
Search Units.
- E 1066, Standard Test Method for Ammonia Colorimetric Leak Testing.
- E 1067, Standard Practice for Acoustic Emission Examination
of Fiberglass Reinforced Plastic Resin (FRP) Tanks/Vessels.
- E 1079, Standard Practice for Calibration of Transmission Densitometers.
- E 1106, Standard Method for Primary Calibration of Acoustic
Emission Sensors.
- E 1114, Standard Test Method for Determining the Focal Size
of Iridium-192 Industrial Radiographic Sources.
- E 1118, Standard Practice for Acoustic Emission Examination
of Reinforced Thermosetting Resin Pipe (RTRP).
- E 1135, Standard Test Method for Comparing the Brightness of
Fluorescent Penetrants.
- E 1139, Standard Practice for Continuous Monitoring of Acoustic
Emission from Metal Pressure Boundaries.
- E 1158, Standard Guide for Material Selection and Fabrication
of Reference Blocks for the Pulsed Longitudinal Wave Ultrasonic
Examination of Metal and Metal Alloy Production Material.
- E 1161, Standard Test Method for Radiologic Examination of Semiconductors
and Electronic Components.
- E 1165, Standard Test Method for Measurement of Focal Spots
of Industrial X-Ray Tubes by Pinhole Imaging.
- E 1208, Standard Test Method for Fluorescent Liquid Penetrant
Examination Using the Lipophilic Post-Emulsification Process.
- E 1209, Standard Test Method for Fluorescent Liquid Penetrant
Examination Using the Water-Washable Process.
- E 1210, Standard Test Method for Fluorescent Liquid Penetrant
Examination Using the Hydrophilic Post-Emulsification Process.
- E 1211, Standard Practice for Leak Detection and Location Using
Surface-Mounted Acoustic Emission Sensors.
- E 1212, Standard Practice for Quality Control Systems for Nondestructive
Testing Agencies.
- E 1213, Standard Test Method for Minimum Resolvable Temperature
Difference for Thermal Imaging Systems.
- E 1219, Standard Test Method for Fluorescent Liquid Penetrant
Examination Using the Solvent-Removable Process.
- E 1220, Standard Test Method for Visible Penetrant Examination
Using the Solvent-Removable Process.
-
E 1254, Standard Guide for Storage of Radiographs
and Unexposed Industrial Radiographic Films.
-
E 1255, Standard Practice for Radioscopy E1316,
Standard Terminology for Nondestructive Examinations.
- E 1311, Standard Test Method for Minimum Detectable Temperature
Difference for Thermal Imaging Systems.
- E 1312, Standard Practice for Electromagnetic (Eddy-Current)
Examination of Ferromagnetic Cylindrical Bar Product Above the
Curie Temperature.
- E 1315, Standard Practice for Ultrasonic Examination of Steel
with Convex Cylindrically Curved Entry Surfaces.
- E 1316, Standard Terminology for Nondestructive Examinations.
- E 1320, Standard Reference Radiographs for Titanium Castings.
- E 1324, Standard Guide for Measuring Some Electronic Characteristics
of Ultrasonic Examination Instruments.
- E 1359, Standard Guide for Evaluating Capabilities of Nondestructive
Testing Agencies.
- E 1390, Standard Guide for Illuminators Used for Viewing Industrial
Radiographs.
- E 1411, Standard Practice for Qualification of Radioscopic Systems.
- E 1416, Standard Test Method for Radioscopic Examination of
Weldments.
- E 1417, Standard Practice for Liquid Penetrant Examination.
- E 1418, Standard Test Method for Visible Penetrant Examination
Using the Water-Washable Process.
- E 1419, Standard Test Method for Examination of Seamless, Gas-
Filled, Pressure Vessels Using Acoustic Emission.
- E 1441, Standard Guide for Computed Tomography (CT) Imaging.
- E 1444, Standard Practice for Magnetic Particle Examination.
- E 1452, Standard Practice for Preparation of Calibration Solutions
for Spectrophotometric and for Spectroscopic Atomic Analysis.
- E 1453, Standard Guide for Storage of Media That Contains Analog
or Digital Radioscopic Data.
- E 1454, Standard Guide for Data Fields for Computerized Transfer
of Digital Ultrasonic Testing Data
- E 1475, Standard Guide for Data Fields for Computerized Transfer
of Digital Radiological Test Data.
- E 1476, Standard Guide for Metals Identification, Grade Verification,
and Sorting.
- E 1495, Standard Guide for Acousto-Ultrasonic Assessment of
Composites, Laminates, and Bonded Joints.
- E 1496, Standard Test Method for Neutron Radiographic Dimensional
Measurements.
- E 1543, Standard Test Method for Noise Equivalent Temperature
Difference of Thermal Imaging Systems.
- E 1570, Standard Practice for Computed Tomographic (CT) Examination.
- E 1571, Standard Practice for Electromagnetic Examination of
Ferromagnetic Steel Wire Rope.
- E 1603, Standard Test Methods for Leakage Measurement Using
the Mass Spectrometer Leak Detector or Residual Gas Analyzer in
the Hood Mode.
- E 1606, Standard Practice for Electromagnetic (Eddy-Current)
Examination of Copper Redraw Rod for Electrical Purposes.
- E 1629, Standard Practice for Determining the Impedance of Absolute
Eddy-Current Probes.
- E 1647, Standard Practice for Determining Contrast Sensitivity
in Radioscopy.
-
E 1648, Standard Reference Radiographs for Examination
of Aluminum Fusion Welds.
-
E 1672, Standard Guide for Computed Tomography
(CT) System Selection.
-
E 1695, Standard Test Method for Measurement
of Computed Tomography (CT) System Performance.
-
E 1734, Standard Practice for Radioscopic Examination
of Castings.
- E 1735, Standard Test Method for Determining Relative Image
Quality of Industrial Radiographic Film Exposed to X-Radiation
from 4 to 25 MV.
- E 1736, Standard Practice for Acousto-Ultrasonic Assessment
of Filament-Wound Pressure Vessels.
- E 1742, Standard Practice for Radiographic Examination.
- E 1774, Standard Guide for Electromagnetic Acoustic Transducers
(EMATs).
- E 1781, Standard Practice for Secondary Calibration of Acoustic
Emission Sensors.
-
E 1814, Standard Practice for Computed Tomographic
(CT) Examination of Castings.
-
E 1815, Standard Test Method for Classification
of Film Systems for Industrial Radiography.
-
E 1816, Standard Practice for Ultrasonic Examinations
Using Electromagnetic Acoustic Transducer (EMAT) Techniques.
- E 1817, Standard Practice for Controlling Quality of Radiological
Examination by Using Representative Quality Indicators (RQIs)
- E 1862-97(2002)e1 Standard Test Methods for Measuring and Compensating
for Reflected Temperature Using Infrared Imaging Radiometers.
- E 1888, Standard Test Method for Acoustic Emission testing of
Pressurized Containers Made of Fiberglass Reinforced Plastic with
Balsa Wood Cores.
- E 1897, Standard Test Methods for Measuring and Compensating
for Transmittance of an Attenuating Medium Using Infrared Imaging.
- E 1901, Standard Guide for Detection and Evaluation of Discontinuities
by Contact Pulse-Echo Straight-Beam Ultrasonic Methods.
- E 1930, Standard Test Method for Examination of Liquid Filled
Atmospheric and Low Pressure Metal Storage Tanks Using Acoustic
Emission.
-
E 1931, Standard Guide for X-Ray Compton Scatter
Tomography.
-
E 1932, Standard Guide for Acoustic Emission
Examination of Small Parts.
- E 1933, Standard Test Methods for Measuring and Compensating
for Emissivity Using Infrared Imaging Radiometers.
- E 1934, Standard Guide for Examining Electrical and Mechanical
Equipment with Infrared Thermography.
- E 1935, Standard Test Method for Calibrating and Meausring
CT Density.
- E 1936, Standard Reference Radiograph for Evaluating the Performance
of Radiographic Digitization Systems.
- E 1955, Standard Radiographic Examination for Soundness of Welds
in Steel by Comparison to Graded ASTM E 390 Reference Radiographs.
- E 1961, Standard Practice for Mechanized Ultrasonic Examination
of Girth Welds Using Zonal Discrimination with Focused Search
Units.
- E1962, Standard Test Method for Ultrasonic Surface Examinations
Using Electromagnetic Acoustic Transducer (EMAT) Techniques.
- E 2001, Standard Guide for Resonant Ultrasound Spectroscopy
for Defect Detection in Both Metallic and Non-Metallic Parts.
- E 2002, Standard Practice for Determining Total Image Unsharpness
in Radiology.
- E 2003, Standard Practice for Fabrication of the Neutron Radiographic
Beam Purity Indicators.
- E 2023, Standard Practice for Fabrication of Neutron Radiographic
Sensitivity Indicators.
- E 2024, Standard Test Methods for Atmospheric Leaks Using a
Thermal Conductivity Leak Detector.
- E 2033, Standard Practice for Computed Radiology (Photostimulable
Luminescence Method).
- E 2075, Standard Practice for Verifying the Consistency of AE-Sensor
Response Using an Acrylic Rod.
- E 2076, Standard Test Method for Examination of Fiberglass Reinforced
Plastic Fan Blades Using Acoustic Emission.
- E 2096, Standard Practice for In Situ Examination of Ferromagnetic
Heat-Exchanger Tubes Using Remote Field Testing.
- E 2104, Standard Practice for Radiographic Examination of Advanced
Aero and Turbine Materials and Components.
- E 2191, Standard Test Method for Examination of Gas-Filled Filament-Wound
Composite Pressure Vessels Using Acoustic Emission.
- E 2192, Standard Guide for Planar Flaw Height Sizing by Ultrasonics.
- E 2223, Standard Practice for Examination of Seamless, Gas-Filled,
Steel Pressure Vessels Using Angle Beam Ultrasonic.
-
F 629, Standard Practice for Radiography of
Cast Metallic Surgical Implants.
-
F 846, Standard Guide for Testing Performance
of Amusement Rides and Devices.
- F 914, Standard Test Method for Acoustic Emission for Insulated
Aerial Personnel Devices.
-
F 1430, Standard Test Method for Acoustic Emission
Testing of Insulated Aerial Personnel Devices with Supplemental
Load Handling Attachments
-
F 1469, Standard Guide for Conducting a Repeatability
and Reproducibility Study on Test Equipment for Nondestructive
Testing.
-
F 1512, Standard Practice for Ultrasonic C-Scan
Bond Evaluation of Sputtering Target-Backing Plate Assemblies.
-
F 1797, Standard Test Method for Acoustic
Emission Testing of Insulated Digger Derricks.
-
G 62, Standard Test Methods for Holiday Detection
in Pipeline Coatings.
-
G 158, Standard Guide for Three Methods of
Assessing Buried Steel Tanks.
-
R0027- Standards Related to Nondestructive Testing
Developed by ASTM Committees Other Than Committee E-7 (This
is not an ASTM standard)

|
|
|