Wood |
Longitudinal Velocity
|
cm/µs |
in/µs |
|
Ash (Along Fiber)
|
0.467 |
0.1839 |
|
Birch (Along Fiber)
|
0.334 |
0.1315 |
|
Cork
|
0.0500 |
0.0197 |
|
Douglas Fir (Cross Grain)
|
0.14 |
0.0551 |
|
Douglas Fir (With Grain)
|
0.480 |
0.189 |
|
Elm (Wood)
|
0.140 |
0.0551 |
|
Maple (Along Fiber)
|
0.411 |
0.1618 |
|
Oak
|
0.447 |
0.176 |
|
Pine (Along Fiber)
|
0.332 |
0.1307 |
|
Poplar (Along Fiber)
|
0.428 |
0.1685 |
|
Sycamore (Along Fiber)
|
0.446 |
0.1756 |
-Data compiled by Xactex Corporation. Sources of original data are unknown.