Examples
of Fluorescent Wet
Magnetic Particle Indications
The indications produced using the wet magnetic
particles are more sharp than dry particle indications formed
on similar defects. When fluorescent particles are used, the visibility
of the indications is greatly improved because the eye is drawn
to the "glowing" regions in the dark setting. Below
are a few examples of fluorescent wet magnetic particle indications.

Magnetic
particle wet fluorescent indication of cracks in a drive shaft.

Magnetic
particle wet fluorescent indication of a crack in a bearing.

Magnetic
particle wet fluorescent indication of a crack in a crane hook.
.jpg)
Magnetic
particle wet fluorescent indication of a crack at a sharp radius.

Magnetic
particle wet fluorescent indication of a crack in a casting.
.jpg)
Magnetic
particle wet fluorescent indication of cracks at a fastener
hole.
|